CASTING DEFECTS 

THE FOLLOWING ARE THE MAJOR DEFECTS, WHICH ARE LIKELY TO OCCUR IN SAND CASTINGS
  •      GAS DEFECTS
  •      SHRINKAGE CAVITIES
  •      MOLDING MATERIAL DEFECTS
  •      POURING METAL DEFECTS
  •      MOLD SHIFT
GAS DEFECTS
A CONDITION EXISTING IN A CASTING CAUSED BY THE TRAPPING OF GAS IN THE MOLTEN METAL OR BY MOLD GASES EVOLVED DURING THE POURING OF THE CASTING. THE DEFECTS IN THIS CATEGORY CAN BE CLASSIFIED INTO BLOWHOLES AND PINHOLE POROSITY. BLOWHOLES ARE SPHERICAL OR ELONGATED CAVITIES PRESENT IN THE CASTING ON THE SURFACE OR INSIDE THE CASTING. PINHOLE POROSITY OCCURS DUE TO THE DISSOLUTION OF HYDROGEN GAS, WHICH GETS ENTRAPPED DURING HEATING OF MOLTEN METAL. 

CAUSES
THE LOWER GAS-PASSING TENDENCY OF THE MOLD, WHICH MAY BE DUE TO LOWER VENTING, LOWER PERMEABILITY OF THE MOLD OR IMPROPER DESIGN OF THE CASTING. THE LOWER PERMEABILITY IS CAUSED BY FINER GRAIN SIZE OF THE SAND, HIGH PERCENTAGE OF CLAY IN MOLD MIXTURE, AND EXCESSIVE MOISTURE PRESENT IN THE MOLD.
  •      METAL CONTAINS GAS
  •      MOLD IS TOO HOT
  •      POOR MOLD BURNOUT
SHRINKAGE CAVITIES
THESE ARE CAUSED BY LIQUID SHRINKAGE OCCURRING DURING THE SOLIDIFICATION OF THE CASTING. TO COMPENSATE FOR THIS, PROPER FEEDING OF LIQUID METAL IS REQUIRED. FOR THIS REASON RISERS ARE PLACED AT THE APPROPRIATE PLACES IN THE MOLD. SPRUES MAY BE TOO THIN, TOO LONG OR NOT ATTACHED IN THE PROPER LOCATION, CAUSING SHRINKAGE CAVITIES. IT IS RECOMMENDED TO USE THICK SPRUES TO AVOID SHRINKAGE CAVITIES. 

MOLDING MATERIAL DEFECTS
THE DEFECTS IN THIS CATEGORY ARE CUTS AND WASHES, METAL PENETRATION, FUSION, AND SWELL.

CUT AND WASHES
THESE APPEAR AS ROUGH SPOTS AND AREAS OF EXCESS METAL, AND ARE CAUSED BY EROSION OF MOLDING SAND BY THE FLOWING METAL. THIS IS CAUSED BY THE MOLDING SAND NOT HAVING ENOUGH STRENGTH AND THE MOLTEN METAL FLOWING AT HIGH VELOCITY. THE FORMER CAN BE TAKEN CARE OF BY THE PROPER CHOICE OF MOLDING SAND AND THE LATTER CAN BE OVERCOME BY THE PROPER DESIGN OF THE GATING SYSTEM.

METAL PENETRATION
WHEN MOLTEN METAL ENTERS INTO THE GAPS BETWEEN SAND GRAINS, THE RESULT IS A ROUGH CASTING SURFACE. THIS OCCURS BECAUSE THE SAND IS COARSE OR NO MOLD WASH WAS APPLIED ON THE SURFACE OF THE MOLD. THE COARSER THE SAND GRAINS MORE THE METAL PENETRATION. 

FUSION
THIS IS CAUSED BY THE FUSION OF THE SAND GRAINS WITH THE MOLTEN METAL, GIVING A BRITTLE, GLASSY APPEARANCE ON THE CASTING SURFACE. THE MAIN REASON FOR THIS IS THAT THE CLAY OR THE SAND PARTICLES ARE OF LOWER REFRACTORINESS OR THAT THE POURING TEMPERATURE IS TOO HIGH.

SWELL
UNDER THE INFLUENCE OF METALLOSTATIC FORCES, THE MOLD WALL MAY MOVE BACK CAUSING A SWELL IN THE DIMENSION OF THE CASTING. A PROPER RAMMING OF THE MOLD WILL CORRECT THIS DEFECT.

INCLUSIONS
PARTICLES OF SLAG, REFRACTORY MATERIALS, SAND OR DEOXIDATION PRODUCTS ARE TRAPPED IN THE CASTING DURING POURING SOLIDIFICATION. THE PROVISION OF CHOKE IN THE GATING SYSTEM AND THE POURING BASIN AT THE TOP OF THE MOLD CAN PREVENT THIS DEFECT. 

POURING METAL DEFECTS
THE LIKELY DEFECTS IN THIS CATEGORY ARE
  •      MIS-RUNS AND
  •      COLD SHUTS.
A MIS-RUN IS CAUSED WHEN THE METAL IS UNABLE TO FILL THE MOLD CAVITY COMPLETELY AND THUS LEAVES UNFILLED CAVITIES. A MIS-RUN RESULTS WHEN THE METAL IS TOO COLD TO FLOW TO THE EXTREMITIES OF THE MOLD CAVITY BEFORE FREEZING.  LONG, THIN SECTIONS ARE SUBJECT TO THIS DEFECT AND SHOULD BE AVOIDED IN CASTING DESIGN.

A COLD SHUT IS CAUSED WHEN TWO STREAMS WHILE MEETING IN THE MOLD CAVITY, DO NOT FUSE TOGETHER PROPERLY THUS FORMING A DISCONTINUITY IN THE CASTING. WHEN THE MOLTEN METAL IS POURED INTO THE MOLD CAVITY THROUGH MORE-THAN-ONE GATE, MULTIPLE LIQUID FRONTS WILL HAVE TO FLOW TOGETHER AND BECOME ONE SOLID.  IF THE FLOWING METAL FRONTS ARE TOO COOL, THEY MAY NOT FLOW TOGETHER, BUT WILL LEAVE A SEAM IN THE PART.  SUCH A SEAM IS CALLED A COLD SHUT, AND CAN BE PREVENTED BY ASSURING SUFFICIENT SUPERHEAT IN THE POURED METAL AND THICK ENOUGH WALLS IN THE CASTING DESIGN.

THE MIS-RUN AND COLD SHUT DEFECTS ARE CAUSED EITHER BY A LOWER FLUIDITY OF THE MOLD OR WHEN THE SECTION THICKNESS OF THE CASTING IS VERY SMALL. FLUIDITY CAN BE IMPROVED BY CHANGING THE COMPOSITION OF THE METAL AND BY INCREASING THE POURING TEMPERATURE OF THE METAL. 

MOLD SHIFT
THE MOLD SHIFT DEFECT OCCURS WHEN COPE AND DRAG OR MOLDING BOXES HAVE NOT BEEN PROPERLY ALIGNED. 

References:- www.nptel.iitm.ac.in/

Comments

Popular posts from this blog

DOM MANUAL / B-TECH / MECHANICAL / KUK - TO FIND THE SPEED AND TORQUE OF DIFFERENT GEARS IN AN EPICYCLIC GEAR TRAIN.

OBJECTIVE: TO FIND THE SPEED AND TORQUE OF DIFFERENT GEARS IN AN EPICYCLIC GEAR TRAIN. SPECIFICATIONS : 1.       GEAR TRAIN : SUN GEAR : 14 TEETH 2.       PLANT GEAR: 21 TEETH (2 NOS.) 3.       INTERNAL GEAR WITH : 56 TEETH TORQUE MEASUREMENT ·          INPUT TORQUE – MOTOR CURRENT CALIBRATED FOR MOTOR TORQUE. ·          PLANT CARRIER - PULLEY OF 50 MM DIA AND SPRING BALANCE. ·          INTERNAL GEAR - PULLEY, 120 MM DIA AND SPRING BALANCES. Ø   BOTH PULLEYS ARE PROVIDED WITH ROPE OF 12 Ø   MM DIA Ø   DRIVE MOTOR - 1HP DC MOTOR RPM MOTOR OPERATING ON 220 VOLTS Ø   50 HZ SUPLLY, DRIVING THE SUN GEAR. CURRENT(AMPS) TORQUE 1.00 0.5 1.20 1.5 1.40 2.5 ...

MANUFACTURING PROCESS - DRAFT OR TAPER ALLOWANCE

DRAFT OR TAPER ALLOWANCE BY DRAFT IS MEANT THE TAPER PROVIDED BY THE PATTERN MAKER ON ALL VERTICAL SURFACES OF THE PATTERN SO THAT IT CAN BE REMOVED FROM THE SAND WITHOUT TEARING AWAY THE SIDES OF THE SAND MOLD AND WITHOUT EXCESSIVE RAPPING BY THE MOLDER. FIGURE  SHOWS A PATTERN HAVING NO DRAFT ALLOWANCE BEING REMOVED FROM THE PATTERN. IN THIS CASE, TILL THE PATTERN IS COMPLETELY LIFTED OUT, ITS SIDES WILL REMAIN IN CONTACT WITH THE WALLS OF THE MOLD, THUS TENDING TO BREAK IT.  FIGURE  IS AN ILLUSTRATION OF A PATTERN HAVING PROPER DRAFT ALLOWANCE. HERE, THE MOMENT THE PATTERN LIFTING COMMENCES, ALL OF ITS SURFACES ARE WELL AWAY FROM THE SAND SURFACE. THUS THE PATTERN CAN BE REMOVED WITHOUT DAMAGING THE MOLD CAVITY.  PATTERN HAVING DRAFT ON VERTICAL EDGES DRAFT ALLOWANCE VARIES WITH THE COMPLEXITY OF THE SAND JOB. BUT IN GENERAL INNER DETAILS OF THE PATTERN REQUIRE HIGHER DRAFT THAN OUTER SURFACES. THE AMOUNT OF DRAFT DEPENDS UPON THE LENGTH OF THE...

ELECTROCHEMICAL MACHINING (ECM)

ELECTROCHEMICAL MACHINING (ECM) INTRODUCTION:- Electro chemical machining (ECM) is a method of removing metal by an electrochemical process. It is normally used for mass production and is used for working extremely hard materials or materials that are difficult to machine using conventional methods. Its use is limited to electrically conductive materials; however, this includes all metals. ECM can cut small or odd-shaped angles, intricate contours or cavities in extremely hard steel and exotic metals such as titanium, carbide etc. ECM is often characterized as "reverse electroplating," and is similar in concept to electrical discharge machining in that a high current is passed between an electrode and the part, through an electrolyte material removal process having a negatively charged electrode (cathode), a conductive fluid (electrolyte), and a conductive work piece (anode); however, in ECM there is no tool wear. The ECM cutting tool is guided along the desired ...